When do drying defects first appear?

The first sighting of a drying check fixes its discovery date. A marked board, a scale and a log of accessible faces give that observation a location and a history. A fresh crosscut can expose a check long after drying is complete. Earlier photographs of the faces alone leave its time of formation open.

A walnut board sketch locates a check against a reference edge and marks one width measurement.
Mark a stable reference edge and return to the same point when measuring a check. Schematic drawing.

Make a map before treatment

Give the board an ID. Label its ends, edges and faces on a sketch. Inspect the accessible surfaces before steaming or drying and photograph existing checks with a scale in the plane of the defect. Assign each check a short ID and mark its visible ends. If a face is hidden in the stack, record it as uninspected.

Measure the same feature twice

Return to each marked location with the same lighting direction and camera angle where practical. If the check curves, choose either its traced length or the straight distance between its visible ends. Record that choice and repeat it at the next inspection.

For an opening-width measurement, mark a specific point along the check and give its distance from the reference edge. A reading at the mouth and another at the tip describe different places. If later trimming removes your reference, photograph the new edge and start a new series.

Date the observation

Identify the last visit when the surface was visible and the first inspection that showed the check. Note any change in surface preparation between those visits. If the defect was inside the board until crosscutting exposed it, the earlier face photographs supply no observation of that interior plane.

Close the entry with information someone else can use to find the defect again: board ID, face or crosscut location, date, photograph and any measured change. Keep a proposed cause alongside the processing history so a later inspection can test it.

Photographs of a pale edge need careful reading before it is labelled a defect. RifleStock’s heartwood and light-edge examples trace a colour boundary across faces. For a German inspection checklist covering the condition of a board before ordering, see Nussbaumqualität vor der Bestellung prüfen.